Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Flow, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Transverse, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.17 mm |
0.017 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm @Thickness 3.17 mm |
0.017 - 0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm @Thickness 3.17 mm |
0.017 - 0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm @Thickness 3.17 mm |
0.017 - 0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Transverse, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 1.27 mm |
0.017 in/in @Thickness 0.0500 in |
Flow; ASTM D955 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Diameter 4.00 mm |
0.017 in/in @Diameter 0.157 in |
Parallel |
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly.. |