Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.016 cm/cm @Thickness 3.20 mm |
0.016 in/in @Thickness 0.126 in |
Normal; DAM; ASTM D955 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.016 - 0.018 cm/cm @Thickness 3.17 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
Direction of Flow; ASTM D955 |
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.016 - 0.018 cm/cm @Thickness 3.17 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
Transverse to Flow; ASTM D955 |
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |