Polymer Property : Linear Mold Shrinkage, Transverse = 0.050 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.020 - 0.050 cm/cm

@Time 86400 sec
0.020 - 0.050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon
LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.030 - 0.050 cm/cm

@Time 86400 sec
0.030 - 0.050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66
LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.030 - 0.050 cm/cm

@Time 86400 sec
0.030 - 0.050 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..