Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.030 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.030 cm/cm

@Time 86400 sec
0.030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP
LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE...
Linear Mold Shrinkage, Transverse 0.030 - 0.050 cm/cm

@Time 86400 sec
0.030 - 0.050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66
LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.030 - 0.050 cm/cm

@Time 86400 sec
0.030 - 0.050 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
E-Polymers TEKASTER® F100 low-mid viscosity PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
E-Polymers TEKASTER® F101F Fast cycle time PBT
Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good..
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties..
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..