Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.017 - 0.029 cm/cm

@Thickness 3.17 mm
0.017 - 0.029 in/in

@Thickness 0.125 in
ASTM D955
Network Polymers Softflex® 0470
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Linear Mold Shrinkage, Transverse 0.021 - 0.029 cm/cm

@Time 86400 sec
0.021 - 0.029 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal
LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 - 0.029 cm/cm

@Time 86400 sec
0.021 - 0.029 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KP004 is a compound based on Acetal Copolymer resin containing PTFE, Silicone.