Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.025 - 0.027 cm/cm @Time 86400 sec |
0.025 - 0.027 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Linear Mold Shrinkage, Transverse | 0.025 - 0.027 cm/cm @Time 86400 sec |
0.025 - 0.027 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.025 - 0.027 cm/cm @Time 86400 sec |
0.025 - 0.027 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.025 - 0.027 cm/cm @Time 86400 sec |
0.025 - 0.027 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.024 - 0.027 cm/cm @Thickness 3.20 mm |
0.024 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 337 PBT Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |