Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0140 - 0.0250 cm/cm
0.0140 - 0.0250 in/in
Average value: 0.0209 cm/cm Grade Count:5
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.0140 - 0.0210 cm/cm
0.0140 - 0.0210 in/in
ISO 294-4
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.0140 - 0.0210 cm/cm
0.0140 - 0.0210 in/in
ISO 294-4
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Linear Mold Shrinkage, Transverse 0.0140 - 0.0160 cm/cm
0.0140 - 0.0160 in/in
ISO 294-4
Celanese CELANEX 4309AR PBT
Celanex 4309AR is a 30% glass reinforced PBT with enhanced resistance to hydrolysis, alkaline environments and salt water spray.Information provided by Celanese
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
ASTM D955
Celanese Celcon® GB25 POM, 25% Glass Reinforced
Celcon« GB25 acetal copolymer is a 25% glass bead filled grade for low shrinkage and warp resistance in large, flat and thin walled parts.Information provided by Celanese
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
ISO 294-4
Celanese Hostaform® LX90Z POM, UV Resistant
Hostaform« LX90Z specialty metallic appearance grades are an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is t..
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
ISO 294-4
Celanese Hostaform® LX90Z XAP² ™ POM, UV Resistant
Preliminary Data SheetInformation provided by Celanese
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
ASTM D955
Celanese Celcon® GC25A POM, 25% Glass Reinforced
Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower..
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
Average value: 0.0140 cm/cm Grade Count:4
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
ISO 294-4
Celanese Celcon® M90AW POM, Tribological
Celcon« M90AW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear in low load-high velocity applications. Celcon« M90AW is an option ..