Polymer Property : Linear Mold Shrinkage, Transverse = 0.0101 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0101 cm/cm

@Time 86400 sec
0.0101 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Transverse 0.0101 cm/cm
0.0101 in/in
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
Linear Mold Shrinkage, Transverse 0.0101 cm/cm

@Time 86400 sec
0.0101 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.