Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0092 cm/cm | 0.0092 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0092 - 0.0094 cm/cm @Time 86400 sec |
0.0092 - 0.0094 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |