Polymer Property : Linear Mold Shrinkage, Transverse = 0.0056 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0056 cm/cm
0.0056 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Linear Mold Shrinkage, Transverse 0.0056 cm/cm
0.0056 in/in
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat..
Linear Mold Shrinkage, Transverse 0.0056 cm/cm
0.0056 in/in
ASTM D955
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Linear Mold Shrinkage, Transverse 0.0056 cm/cm
0.0056 in/in
ISO 294-4
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
Linear Mold Shrinkage, Transverse 0.0056 cm/cm

@Time 86400 sec
0.0056 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific)
This material is mineral filled PPO grade with high dielectric constant and low loss tangent
Linear Mold Shrinkage, Transverse 0.0056 cm/cm
0.0056 in/in
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling
FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C..