Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00592 cm/cm Grade Count:24
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00545 cm/cm Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0110 cm/cm
0.00900 - 0.0110 in/in
Average value: 0.00967 cm/cm Grade Count:3
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Linear Mold Shrinkage, Transverse 0.00190 - 0.0110 cm/cm
0.00190 - 0.0110 in/in
Average value: 0.00698 cm/cm Grade Count:5
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00708 cm/cm Grade Count:6
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage, Transverse 0.00330 - 0.0110 cm/cm
0.00330 - 0.0110 in/in
Average value: 0.00903 cm/cm Grade Count:37
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0110 cm/cm
0.00500 - 0.0110 in/in
Average value: 0.00792 cm/cm Grade Count:13
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00600 cm/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00555 cm/cm Grade Count:47
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00788 cm/cm Grade Count:10
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0110 cm/cm
0.00800 - 0.0110 in/in
Average value: 0.00958 cm/cm Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..