Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | -0.00300 - 0.00900 cm/cm | -0.00300 - 0.00900 in/in | Average value: 0.00457 cm/cm Grade Count:22 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | -0.00300 - 0.0080 cm/cm | -0.00300 - 0.0080 in/in | ASTM D955 |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |