Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5000 - 8000 cP @Shear Rate 250 1/s, Temperature 25.0 °C |
5000 - 8000 cP @Shear Rate 250 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2110309D5 Carbon Graphite Ink This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is formulated to give superior printing properties with good definition for fine line printing.Produ.. |
|||
Viscosity | 5500 - 8000 cP @Temperature 77.0 °C |
5500 - 8000 cP @Temperature 171 °F |
|
Dow VORALUX™ HL 430 Copolymer Polyol VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan.. |
|||
Viscosity | 4000 - 8000 cP @Temperature 25.0 °C |
4000 - 8000 cP @Temperature 77.0 °F |
Part B; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |