Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 4000 - 5000 cP

@Temperature 25.0 °C
4000 - 5000 cP

@Temperature 77.0 °F
TA4302A
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Viscosity 4000 - 5000 cP

@Temperature 25.0 °C
4000 - 5000 cP

@Temperature 77.0 °F
TA4302B
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Viscosity 4000 cP

@Temperature 25.0 °C
4000 cP

@Temperature 77.0 °F
STM 1
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o..
Viscosity 4000 - 8000 cP

@Temperature 25.0 °C
4000 - 8000 cP

@Temperature 77.0 °F
Part B; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and ..