Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 52700 cP @Shear Rate 1340 1/s, Temperature 200 °C |
52700 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |