Polymer Property : Viscosity = 52700 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 52700 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
52700 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav..