Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 46800 cP @Shear Rate 1340 1/s, Temperature 200 °C |
46800 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Viscosity | 46800 cP @Shear Rate 5000 1/s, Temperature 280 °C |
46800 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |