Polymer Property : Viscosity = 46800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 46800 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
46800 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Viscosity 46800 cP

@Shear Rate 5000 1/s,
Temperature 280 °C
46800 cP

@Shear Rate 5000 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers