Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 34000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
34000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |
|||
Viscosity | 34000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
34000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 .. |
|||
Viscosity | 34000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
34000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Viscosity | 34000 cP @Temperature 17.0 °C |
34000 cP @Temperature 62.6 °F |
|
Lendell Manufacturing Prepol Pre Polymer Liquid Apperance, Amber, honey likePolyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 8.. |