Dow LDPE 722M Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 722M Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include caps/closures. This resin has good processability over a wide range of molding conditions. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
Viscosity 34000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
34000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
76000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
130000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
130000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 8.0 g/10 min

@Load 2.16 kg
8.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 9.3.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Tensile Strength, Yield 8.90 MPa
1290 psi
Elongation at Break 130 %
130 %
Modulus of Elasticity 0.139 GPa
20.2 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.226 GPa
32.8 ksi
Izod Impact, Notched (ISO) 28.0 kJ/m²

@Temperature -50.0 °C
13.3 ft-lb/in²

@Temperature -58.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F