Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 27 cP @Temperature 30.0 °C |
27 cP @Temperature 86.0 °F |
5% wt Toluene Solution |
Kuraray SEPTON® S2006 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Viscosity | 27 cP @Shear Rate 1000 1/s, Temperature 290 °C |
27 cP @Shear Rate 1000 1/s, Temperature 554 °F |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Viscosity | 27 cP @Temperature 60.0 °C |
27 cP @Temperature 140 °F |
|
BASF Pluracol® P710R Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Viscosity | 27 cP @Temperature 40.0 °C |
27 cP @Temperature 104 °F |
Absolute |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |