Material Notes:
Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with Pluracol 2097 in combination with graft polyols, such as Pluracol 4830, process well and are easily crushed. Pluracol 2097 is less reactive than either Pluracol 816 or Pluracol 945.Information provided by BASF
Physical Properties Metric English Comments
Density 0.990 g/cc

@Temperature 55.0 °C
0.0358 lb/in³

@Temperature 131 °F
0.999 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
1.01 g/cc

@Temperature 25.0 °C
0.0365 lb/in³

@Temperature 77.0 °F
Viscosity 210 cP

@Temperature 55.0 °C
210 cP

@Temperature 131 °F
400 cP

@Temperature 40.0 °C
400 cP

@Temperature 104 °F
840 cP

@Temperature 25.0 °C
840 cP

@Temperature 77.0 °F
Molecular Weight 4800 g/mol
4800 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <50
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 34 - 36 mg KOH/g
STI 3007/3162
Unsaturation <0.06 meq/g
STI 3056