Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 153000 cP @Shear Rate 500 1/s, Temperature 250 °C |
153000 cP @Shear Rate 500 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Viscosity | 153000 cP @Shear Rate 300 1/s, Temperature 190 °C |
153000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |