Physical Properties Metric English Comments
Viscosity 153000 cP

@Shear Rate 500 1/s,
Temperature 250 °C
153000 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..
Viscosity 153000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
153000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ IP-10262 High Density Polyethylene
DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a..