Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 135 cP @Shear Rate 100 1/s, Temperature 300 °C |
135 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Viscosity | 135 cP @Shear Rate 100 1/s, Temperature 300 °C |
135 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 135 cP @Shear Rate 100 1/s, Temperature 300 °C |
135 cP @Shear Rate 100 1/s, Temperature 572 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 135 cP @Shear Rate 300 1/s, Temperature 230 °C |
135 cP @Shear Rate 300 1/s, Temperature 446 °F |
Apparent viscosity; ASTM D3835 |
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **) Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,.. |