Material Notes:
Description: Pluracol® 3042 polyol is 41 hydroxyl number (nominal 4000 molecular weight) propoxylated polyether.Information provided by BASF
Physical Properties Metric English Comments
Density 0.992 g/cc

@Temperature 70.0 °C
0.0358 lb/in³

@Temperature 158 °F
1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
1.01 g/cc

@Temperature 25.0 °C
0.0365 lb/in³

@Temperature 77.0 °F
Viscosity 102 cP

@Temperature 70.0 °C
102 cP

@Temperature 158 °F
322 cP

@Temperature 40.0 °C
322 cP

@Temperature 104 °F
724 cP

@Temperature 25.0 °C
724 cP

@Temperature 77.0 °F
Molecular Weight 4000 g/mol
4000 g/mol
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <50
APHA, STI 3057
Colorless Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 39.5 - 42.5 mg KOH/g
STI 3007/3162
Unsaturation <0.05 meq/g