Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Nye Lubricants 701 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Nye Lubricants 782KA (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Nye Lubricants 782LC (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Nye Lubricants 802-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Nye Lubricants 855D (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M30 Series Mobilgard M30 Series (M330 and M430) by ExxonMobil are premium, extra high performance 30 TBN engine oils designed for use in the most severe residual-fueled, medium-speed diesel engines used in mar.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M50 Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M40 Series Mobilgard M40 Series (M340 and M440) by ExxonMobil are premium, extra high performance 40 TBN engine oils designed for use in the most severe residual-fuelled medium-speed diesel applications found .. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil |
ConocoPhillips Tacna® 2000 NLGI No. 2 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Havoline® SAE 80W-90 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ChevronTexaco MP Drive Train Fluid FeaturesChevron Drive Train Fluid - MP is a multipurpose lubricant designed for use in transmissions, wet brakes, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or TO-4M requiremen.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 40 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Taro® 16 XD SAE 40 Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Taro® 20 DP SAE 40 Texaco Taro 20 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Taro® 30 DP SAE 40 Texaco Taro 30 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Taro® 40 XL SAE 40 Texaco Taro 40 XL delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Taro® 50 XL SAE 40 Texaco Taro 50 XL delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Texmar 16 SG SAE 40 Texaco Texmar 16 SG delivers value through:Wear protection — Texaco Texmar 16 SG oil has superior anti-wear characteristics to reduce wear on all moving engine components. Controls ring and liner w.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M30 Series Mobilgard M30 Series (M330 and M430) by ExxonMobil are premium, extra high performance 30 TBN engine oils designed for use in the most severe residual-fueled, medium-speed diesel engines used in mar.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M40 Series Mobilgard M40 Series (M340 and M440) by ExxonMobil are premium, extra high performance 40 TBN engine oils designed for use in the most severe residual-fuelled medium-speed diesel applications found .. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M50 Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ConocoPhillips El Mar® 2000 Oil SAE Grade 15W-40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | |
ChevronTexaco Havoline® SAE 40 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |
|||
Kinematic Viscosity at 100°C (212°F) | 14 cSt | 14 cSt | Base Oil; ASTM D445 |
Chesterton 635 SXC Synthetic, Extreme Pressure & Corrosion Resistant Grease Description: Chesterton® Synthetic Extreme Pressure & Corrosion Resistant Grease is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse with outstanding .. |