Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 716B (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 793 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 822S-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | ASTM D445 |
ChevronTexaco B Soluble Oil FeaturesChevron Soluble Oils are used broadly in machine shops as multifunctional cutting fluids. They are primarily designed to cool and lubricate the contact point of the tool and the work piece.C.. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | |
ELM® SoyFluid™ Hydraulic Food Grade Biodegradable – Biobased Hydraulic Oil Description: ELM SoyFluid™ Hydraulic Food Grade is a biodegradable hydraulic oil formulated with optimized USA-grown natural seed oil that surpasses the lubricity of most conventional oils. It is f.. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | ASTM D445 |
ExxonMobil Exterex™ P61 Synthetic Fluid Product Description: Esterex™ Phthalate Esters are API category Group V fluids. Esterex™ Phthalate Esters have excellent lower-temperature properties, good lubricating properties and low volatilit.. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | ASTM D445 |
ChevronTexaco NB Soluble Oil FeaturesChevron Soluble Oils are used broadly in machine shops as multifunctional cutting fluids. They are primarily designed to cool and lubricate the contact point of the tool and the work piece.C.. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | ASTM D445 |
ChevronTexaco Drive Train Fluid HD, SAE 10W FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | |
ChevronTexaco Soluble D Texaco Soluble Oil D delivers value through:No separation — Excellent emulsion even with hard waterRust protection for steel work and machined parts even when water-oil emulsion ratios are eighty t.. |
|||
Kinematic Viscosity at 40°C (104°F) | 38 cSt | 38 cSt | |
ChevronTexaco SAE 10W Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |