ELM® SoyFluid™ Hydraulic Food Grade Biodegradable – Biobased Hydraulic Oil

Category Fluid , Lubricant
Manufacturer ELM®
Trade Name SoyFluid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELM® SoyFluid™ Hydraulic Food Grade Biodegradable – Biobased Hydraulic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ELM SoyFluid™ Hydraulic Food Grade is a biodegradable hydraulic oil formulated with optimized USA-grown natural seed oil that surpasses the lubricity of most conventional oils. It is formulated in accordance with the criteria established by the USDA for H-1 lubricants and U.S. FDA Regulation 21 CFR 178.3570, “Lubricants With Incidental Food Contact.” Applications: Specifically formulated to meet the demanding applications of major food and meat processing plants.Excellent for large or small cylinders, motors and hydraulic components. Ideal for general hydraulic near water or in environmentally sensitive applications. Wherever USDA H-1 Hydraulic Oils are specified Benefits: Superior lubricity promotes long equipment lifeProtects pumps, valves, cylinders and other components from wear.Protects all ferrous metal components from rust and corrosion.Biodegradable formula is mostly benign if released in environment Compatible with most hydraulic hoses and seals Has superior flash and fire points for increased safety Meets USDA’s proposed Biobased product definition for EO 13101 Meets EPA’s Environmental Preferable Purchasing (EPP) criteria Made from renewable USA-grown crop-based oils Meets State of Iowa Senate File - SF 2185 and 2249 Information provided by ELM®
Physical Properties Metric English Comments
Viscosity Measurement 38
38
ISO
223
223
Index
Kinematic Viscosity at 40°C (104°F) 38 cSt
38 cSt
Thermal Properties Metric English Comments
Pour Point -10.0 °C
14.0 °F
Flash Point 256 °C
493 °F
Descriptive Properties Value Comments
Rust & Corrosion 1A
ASTM D130