ConocoPhillips 2 Super Lube M EP Grease NLGI No.

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 2 Super Lube M EP Grease NLGI No..pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road equipment manufactured by Caterpillar, Komatsu-Dresser, J.I. Case, John Deere and others. These include bulldozers, scrapers, off-highway trucks, wheel loaders, pipelayers, skidders, motor graders and soil compactors where the chassis components and wheel bearings are subjected to heavy loading. Super Lube M EP Grease is also recommended for use in automotive and commercial applications such as chassis, wheel bearings, water pump bearings, universal joints, constant velocity joints, brake self-adjusting screws, tractor-trailer fifth wheels and clutch release bearings. Super Lube M EP Grease also can be used in heavily loaded antifriction and plain bearings used in gear boxes and electric motors. These are commonly found in steel, chemical and aluminum manufacturing plants, where the manufacturer specifies a lithium or lithium complex EP corrosion-resistant grease with moly.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 200 cSt
200 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 14.5 cSt
14.5 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 60
60
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
Four Ball Wear 0.460 mm
0.0181 in
Penetration P(60), 1/10 mm 280
280
Timken Test 27200 g
60.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 191 °C
375 °F
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Dropping Point >= 260 °C
>= 500 °F
Descriptive Properties Value Comments
ASTM Rust Fresh and Saltwater Pass
Color Gray-Black
Molybdenum Disulfide 3 wt.%
Oil Separation 0.21 wt.% Loss
Oxidation Stability 7 psi drop/100 hrs
Roll Stability 4.2% change in consistency
Soap Type (Thickener) Lithium Complex
Water Washout 1.6 %
175°F