Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | |
ChevronTexaco Taro® 16 XD SAE 40 Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | |
ChevronTexaco Texmar 16 SG SAE 40 Texaco Texmar 16 SG delivers value through:Wear protection — Texaco Texmar 16 SG oil has superior anti-wear characteristics to reduce wear on all moving engine components. Controls ring and liner w.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Kinematic Viscosity at 40°C (104°F) | 132 cSt | 132 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |