ExxonMobil Mobil Pegasus 701 Series 40

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Pegasus 701 Series 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and economy for a wide variety of engine types, service severity and fuel quality. Mobil Pegasus 701 and 701 SAE 30 are formulated with ashless dispersants, effective oxidation and corrosion inhibitors, and antiwear agents. They provide excellent dispersancy, and good high-temperature stability. The formulation approach is very effective for controlling carbon and ash deposits in gas engines. The ashless dispersants in Mobil Pegasus 701 and SAE 30 help prevent the formation of deposits that can cause detonation. Port carbon cleaning intervals in two-cycle, naturally aspirated and turbocharged gas engines may be extended by using Pegasus 701 Series oils. Mobil Pegasus 701 Series has increased engine overhaul periods and oil filter and spark plug life in both four-cycle and two-cycle gas engines.Crankcases and power cylinders of spark-ignited two- and four-cycle gas engines; High speed two-cycle gas engines; Suitable for use in modern two-cycle and four-cycle slow-speed gas engines except where severity of application requires special heavy-duty, load-carrying performance; Highly loaded 4-cycle engines requiring anti-scuff protection; Reciprocating compressor cylinders compressing natural gas; High output or naturally aspirated turbocharged engines operating at or in excess of rated capacity under high temperatures
Physical Properties Metric English Comments
Density 0.885 g/cc

@Temperature 15.0 °C
0.0320 lb/in³

@Temperature 59.0 °F
ASTM D1298
Viscosity Measurement 97
97
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 132 cSt
132 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 13.5 cSt
13.5 cSt
ASTM D445
Ash <= 0.070 %
<= 0.070 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
ASTM D97
Flash Point 249 °C
480 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 2.2
2.2
mgKOH/g; ASTM D2896