Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 32
32
ISO Grade
113
113
Viscosity Index
Saybolt Viscosity at 100°F 152 SUS
152 SUS
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt
32 cSt
Kinematic Viscosity at 100°C (212°F) 5.0 cSt
5.0 cSt
Thermal Properties Metric English Comments
Pour Point -23.3 °C
-10.0 °F
Flammability Test 440
440
[°F] Fire Point
Flash Point 199 °C
390 °F
Descriptive Properties Value Comments
SAE No. 10