Material Notes:
Silvaloy X55 has excellent gap filling capability and plasticity when in the molten condition. It also exhibits excellent strength and ductility while cooling from the liquid stage. The improved strength and ductility at elevated temperatures gives it the added advantage over nickel silvers in joining materials with dissimilar coefficient of expansion.The primary application is in the joining of carbides to steel holders. This application requires an alloy with good gap filling characteristics as well as superior toughness and ductility at elevated temperatures.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.35 g/cc
8.35 g/cc
Density 8.33 g/cc
0.301 lb/in³
Thermal Properties Metric English Comments
Melting Point 866 - 885.0 °C
1590 - 1625 °F
Solidus 866 °C
1590 °F
Liquidus 885.0 °C
1625 °F
Component Elements Properties Metric English Comments
Copper, Cu 54 - 56 %
54 - 56 %
Manganese, Mn 3.25 - 4.75 %
3.25 - 4.75 %
Nickel, Ni 5.25 - 6.75 %
5.25 - 6.75 %
Zinc, Zn 32.5 - 37.5 %
32.5 - 37.5 %
As balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000160 ohm-cm
0.0000160 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 899 - 1010 °C
1650 - 1850 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 10.8