Physical Properties Metric English Comments
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 9H0600A
LNP* Thermocomp* 9H0600A is a High Specific Gravity compound containing proprietary fillers.
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 1050CO94 Copper Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityCopper Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding
Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing..
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 1700CO94 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech..
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 705ZG91 Stainless Steel/Tungsten Filled ABS
High Specific GravityStainless Steel/Tungsten Powder Filled ABSInformation provided by Technical Polymers
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Ecomass® 720ZD88 Tungsten Filled ABS
High Specific GravityTungsten Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches