Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 5.90 g/cc | 5.90 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |