Physical Properties Metric English Comments
Specific Gravity 5.90 g/cc
5.90 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6
LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.