Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.30 - 4.50 g/cc | 4.30 - 4.50 g/cc | |
Reade Advanced Materials Iron Chromite (FeO·Cr2O3) A key source of chromium. The general specification is: SFSA 16T-67. A source of chromium metal, chromium chemicals, pigment, refractory mortars, and used as foundry sand.Information provided by Re.. |
|||
Specific Gravity | 4.30 g/cc | 4.30 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Specific Gravity | 4.30 g/cc | 4.30 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Specific Gravity | 4.30 g/cc | 4.30 g/cc | |
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide This grade is made up of > 80% alumina and the balance yttria stabilized zirconia (Y-TZP). Provides some of the advantages of pure Y-TZP at a reduced price. The addition of zirconia increases greatl.. |