Polimersan Plastics POLITEF® (PTFE) with 60% Bronze

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimersan Plastics POLITEF® (PTFE) with 60% Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical ConductivityIncrease At Corrosion ResistanceIncrease In Deformation Strength Against Load Decrease In Thermal ExpansionHigh Resistance Against AcidsEasiness At Mechanical Processing StretchingResistance Against StrokeIncrease In Thermal Conductivity Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.
Physical Properties Metric English Comments
Specific Gravity 3.80 - 4.00 g/cc
3.80 - 4.00 g/cc
ASTM D1457-18
Deformation 5.0 - 5.5 %
5.0 - 5.5 %
230°C, 1 day, 140 kg/cm^2; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 63 - 70
63 - 70
ASTM D2240
Tensile Strength, Yield 16.7 - 17.2 MPa
2420 - 2490 psi
ASTM D1708
Elongation at Break 170 - 180 %
170 - 180 %
ASTM D1708
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
44.4 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Thermal Conductivity 0.96462 W/m-K
6.6836 BTU-in/hr-ft²-°F
ASTM C177
Descriptive Properties Value Comments
Corrosion 10 - 15 cc-dak/kg-ms
25 - 1000°C
Kinding Temperature 640
°C, ASTM D1929