CIMBAR CIMTUFF® 9103s Talc

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name CIMTUFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR CIMTUFF® 9103s Talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CIMTUFF® 9103s talc is a treated talc produced from high purity ore, which provides low iron content, low surface area and superior color in dry form as well as when incorporated with resins. CIMTUFF® 9103s talc is primarily used in appearance and natural polypropylene, where improved tensile strength, flexural modulus, heat distortion temperature, increased stiffness, reduced shrinkage and lower compounding costs are required. The low level amino functional silane treatment helps aid dispersion and couple the mineral with various resin systems, most notably polyolefins. CIMTUFF® 9103s talc is platy, hydrophobic, non-abrasive and chemically inert.9103s talc industrial applications include: thermoplastics, thermosets, TPOs, TPEs rubber compounds, adhesives, sealants and paints & coatings.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Bulk Density 0.256 g/cc
0.00926 lb/in³
Loose
0.721 g/cc
0.0260 lb/in³
Tapped
Brightness 92 %
92 %
Hunter Y, Rd Value, dry
Oil Absorption 38 %
38 %
g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Loss On Ignition 6.0 %
6.0 %
Particle Size 3.8 µm
3.8 µm
Median
pH 8.7
8.7
Mechanical Properties Metric English Comments
Hardness, Mohs 1.0
1.0
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 30 %
30 %
SiO2 60 %
60 %