Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.62 g/cc | 2.62 g/cc | |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Specific Gravity | 2.62 g/cc | 2.62 g/cc | |
Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film streng.. |
|||
Specific Gravity | 2.62 g/cc | 2.62 g/cc | |
Silberline SilBerCote® PC 1291X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.62 g/cc | 2.62 g/cc | |
Silberline SilBerCote® PC 3331X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.62 g/cc @Temperature 25.0 °C |
2.62 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4490 CV One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning |