Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay

Category Ceramic , Clay , Kaolin Clay
Manufacturer Old Hickory Clay Co.
Trade Name M&M Clays, Inc.
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film strength to ceramic engobes and glazes of all temperature ranges. Wilco UPF also meets the requirements of filler applications where a dry ground processed kaolin can be employed.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Specific Gravity 2.62 g/cc
2.62 g/cc
Bulk Density 3.59 g/cc
0.130 lb/in³
Moisture Absorption <= 1.00 %
<= 1.00 %
Particle Size 0.50 µm
0.50 µm
32.2% of particles less than
1.0 µm
1.0 µm
46.4% of particles less than
1.3 µm
1.3 µm
Median particle diameter
2.0 µm
2.0 µm
57.4% of particles less than
5.0 µm
5.0 µm
73.3% of particles less than
10 µm
10 µm
85.1% of particles less than
<= 20 µm
<= 20 µm
91.1% of particles less than
pH 4.5 - 6.5
4.5 - 6.5
10% solids
Specific Surface Area 17 m²/g
17 m²/g
Brookfield Viscosity 1000 cP
1000 cP
70% solids dispersed using a Brookfield #3 spindle at 100 rpm
Component Elements Properties Metric English Comments
Al2O3 37.77 %
37.77 %
CaO 0.10 %
0.10 %
Fe2O3 0.67 %
0.67 %
K2O 0.22 %
0.22 %
Loss on Ignition(%) 13.18 %
13.18 %
MgO 0.050 %
0.050 %
Na2O 0.030 %
0.030 %
SiO2 45.81 %
45.81 %
TiO2 1.74 %
1.74 %
Descriptive Properties Value Comments
CEC/MBI (meg/100 ml) 3.5
Pyrometric Cone Equivalent (PCE) 34
Wet Sieve Residue (%) 1
Wet Sieve Residue, +325 mesh