Physical Properties Metric English Comments
Specific Gravity 2.30 - 2.40 g/cc

@Temperature 25.0 °C
2.30 - 2.40 g/cc

@Temperature 77.0 °F
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive
Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther..
Specific Gravity 2.20 - 2.40 g/cc
2.20 - 2.40 g/cc
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..
Copyright © lookpolymers.com All Rights Reserved