Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

St. Cloud Natural Zeolite (Clinoptilolite)

Category Ceramic , Oxide , Silicon Oxide
Manufacturer St. Cloud Mining Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF St. Cloud Natural Zeolite (Clinoptilolite).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large internal surface area in the porous structure and exchangable cations lead to a variety of uses. It is used as an animal feed supplement that has been shown to improve health and reduce the negative effects of animal waste; as an additive to animal stalls and pens to reduce ammonia and other emissions to air and water; as a soil amendment to retain water and plant nutrients in root zones, which conserves both; for a number of other horticultural and agricultural uses, including being endorsed for use in space by NASA; as a water filtration media that removes ammonia, some heavy metals and other constituents; etc.Major exchangeable cations are Rb, Li, K, Cs, NH4, Na, Ca, Ag, Cd, Pb, Zn, Ba, Sr, Cu, Hg, Mg, Fe, Co, Al, Cr. Primary adsorbing gases are CO, CO2, SO2, H2S, NH3, HCHO, Ar, O2, N2, H2O, He, H2, Kr, Xe, CH2OH, Freon, formaldehyde, and mercaptans.Product mined near Winston, New Mexico, USA.Information provided by St. Cloud Mining Company.
Physical Properties Metric English Comments
Specific Gravity 2.20 - 2.40 g/cc
2.20 - 2.40 g/cc
Bulk Density 0.705 - 0.769 g/cc
0.0255 - 0.0278 lb/in³
Aggregate, dried, 4 x 6 mesh
0.721 - 0.753 g/cc
0.0260 - 0.0272 lb/in³
Aggregate, dried, 6 x 14 mesh
0.737 - 0.785 g/cc
0.0266 - 0.0284 lb/in³
Aggregate, dried, 14 x 40 mesh
0.769 - 0.833 g/cc
0.0278 - 0.0301 lb/in³
Aggregate, dried, -40 mesh
1.39 g/cc
0.0503 lb/in³
In Place, dried
Porosity <= 52 %
<= 52 %
Natural Internal Porosity
pH 7.5 - 8.0
7.5 - 8.0
Natural
Specific Surface Area 14 - 15 m²/g
14 - 15 m²/g
External
<= 800 m²/g
<= 800 m²/g
Total
Permeability 0.001
0.001
m/sec (1.4 - 0.4 mm particles)
Pore Size 0.000400 - 0.000700 microns
0.0000157 - 0.0000276 mil
4 - 7 angstroms Diameter
Mechanical Properties Metric English Comments
Hardness, Mohs 3.5 - 4.0
3.5 - 4.0
Compressive Strength 17.2 MPa
2500 psi
crush strength
Abrasion 24
24
LA Wear
Thermal Properties Metric English Comments
Decomposition Temperature 650 °C
1200 °F
Optical Properties Metric English Comments
Reflection Coefficient, Visible (0-1) 0.85
0.85
Component Elements Properties Metric English Comments
Al2O3 12.1 %
12.1 %
CaO 3.4 %
3.4 %
Fe2O3 1.6 %
1.6 %
K2O 3.0 %
3.0 %
MgO 1.5 %
1.5 %
Na2O 0.3 %
0.3 %
P2O5 0.05 %
0.05 %
SiO2 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 9000 ohm-cm
9000 ohm-cm
Descriptive Properties Value Comments
Cation Exchange Capacity 0.1 meq/g external
0.8 – 1.2 meq/g total
Clinoptilolite Content 75 to 85%
Color White
Feature free flowing
non-slaking
non-soluble
readily mixable
pH Stability 0 - 13
Si:Al Ratio 5:1
Surface Charge Density 10.1E-23 meq/Ã…2
Swelling Index nil