Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.15 - 2.24 g/cc | 2.15 - 2.24 g/cc | ASTM D792 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
Specific Gravity | 2.17 - 2.24 g/cc | 2.17 - 2.24 g/cc | ASTM D792 |
Isoflon PTFE + 3% MoS2 Polytetrafluoroethylene with 3% Molybdenum disulfide Properties:Low coefficient of friction (static)Good thermal conductivityImproved wear resistanceOften combined with glass and bronzeApplications: Specially used for non-lubricated seals with period.. |