Material Notes:
General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApplicationsSemiconductorChemical ProcessingFoodPharmaceuticalAerospaceTelecommunicationsInformation provided by Technetics Group (formerly Plastomer Technologies)
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.24 g/cc
2.15 - 2.24 g/cc
ASTM D792
Deformation 3.0 - 9.0 %
3.0 - 9.0 %
73°F., 2000 psi, 24 hrs.; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 58
55 - 58
ASTM D2240
Tensile Strength, Yield 6.89 - 13.8 MPa
1000 - 2000 psi
ASTM D1708
Elongation at Yield 50 - 150 %
50 - 150 %
ASTM D1709
Compressive Strength 6.21 - 8.27 MPa
900 - 1200 psi
@ 1.0% Strain; ASTM D695
8.27 - 11.0 MPa
1200 - 1600 psi
@ 0.2% Offset; ASTM D695
Thermal Properties Metric English Comments
CTE, linear 54.0 - 144 µm/m-°C

@Temperature 25.6 - 204 °C
30.0 - 80.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Thermal Conductivity 0.360 - 0.504 W/m-K
2.50 - 3.50 BTU-in/hr-ft²-°F
ASTM C-177