Polymer Property : Specific Gravity = 2.17 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.17 g/cc
2.17 g/cc
ASTM D4895
3M Dyneon™ TFX 2035 PTFE  (discontinued **)
Typical Applications: Liners, extruded tape, thick wall tubing.Information provided by the Dyneon division of 3M.
Specific Gravity 2.17 - 2.24 g/cc
2.17 - 2.24 g/cc
ASTM D792
Isoflon PTFE + 3% MoS2 Polytetrafluoroethylene with 3% Molybdenum disulfide
Properties:Low coefficient of friction (static)Good thermal conductivityImproved wear resistanceOften combined with glass and bronzeApplications: Specially used for non-lubricated seals with period..
Specific Gravity 2.17 - 2.23 g/cc
2.17 - 2.23 g/cc
ASTM D 792
Karina 1000/2065-IE MBPEB White (DT) Color Concentrate
Filled white color concentrate recommended for polyolefins applications.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 2.17 - 2.23 g/cc
2.17 - 2.23 g/cc
ASTM D 792
Karina E 1000/3055-IE MBPEB White Color Concentrate
TIO2+ mineral concentrate recommended for polyolefins application (films, packaging, bags, etc.).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 2.17 g/cc
2.17 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Specific Gravity 2.17 g/cc
2.17 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP)
LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers.
Specific Gravity 2.17 g/cc

@Temperature 25.0 °C
2.17 g/cc

@Temperature 77.0 °F
Dow Corning SE 4422 SILICONE RTV
One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning
Specific Gravity 2.17 g/cc
2.17 g/cc
Asahi Glass Fluon® CD145 PTFE Coagulated Dispersion Powder
Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc.