Material Notes:
TIO2+ mineral concentrate recommended for polyolefins application (films, packaging, bags, etc.).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 2.17 - 2.23 g/cc
2.17 - 2.23 g/cc
ASTM D 792
Moisture Absorption <= 0.100 %
<= 0.100 %
ME-52
Ash 83 - 87 %
83 - 87 %
CaCO<sub>3</sub>, ME 51
Descriptive Properties Value Comments
Application Extrusion
Dispersion OK
ME 56
Granulomety 20 - 30
grains/g; ME 05
Pellet Form OK