Material Notes:
Filled white concentrate recommended for olefin applications. Recommended usage from 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 2.09 - 2.15 g/cc
2.09 - 2.15 g/cc
ASTM D 792
Moisture Absorption <= 0.100 %
<= 0.100 %
ME-52
Ash 83 - 87 %
83 - 87 %
CaCO<sub>3</sub>, ME 51
ASTM Color <= 1.0
<= 1.0
Color - Delta E, ME 12
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Heat Resistance; DIN 53772
Descriptive Properties Value Comments
Application Extrusion
Dispersion OK
ME 56
Granulomety 20 - 30
grains/g; ME 05
Lightfastness 8
Scale: 1 to 8
Migration Resistance 5
Scale: 1 to 5
Recommended Application (%) 5
Copyright © lookpolymers.com All Rights Reserved