Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Specific Gravity | 1.64 - 1.70 g/cc | 1.64 - 1.70 g/cc | ASTM D 792 |
Karina 18/219-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Daelim H&L Plavis-G40 CM 40% Graphite Filled Aromatic Polyimide Bearing Compression Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbo.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio.. |
|||
Specific Gravity | 1.64 g/cc @Temperature 25.0 °C |
1.64 g/cc @Temperature 77.0 °F |
|
Dow Corning 236 DISPERSION Flowable (as supplied) silicone RTV coatingInformation provided by Dow Corning |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |